1, the bottle mouth flash
The
edge of the bottle mouth refers to the thread at the mouth of the
bottle or the material at the closed part of the mold constitutes a thin
layer of protrusion. Usually the mold wear constitutes the mold closure
is not accurate, which constitutes too much data injection molding,
showing the appearance of the flash.
2, poor mold clamping
Poor
clamping results in poor mold clamping and poor blow molding. The
reason for its composition is similar to that of the bottle burrs due to
the wear of the mold.
3, the dark ring
There is surplus
information on the shoulder of the bottle, and I want a ring to be
embedded there. The reason for its formation is usually due to uneven
heating and rotation, and uneven stretching data during blow molding.
4, there are impurities
There
are impurities, black spots, foreign matter, unablated particle
particles, etc. in the bottle of the blow molding machine. The reason
for the composition is usually that there is doubt about the disposal of
the data before the injection molding machine. For example, if the mold
part is clean, there will be black spots on the bottle. If the data
particles are not pure, the foreign matter will be present, and the
ablation will be incomplete. The filter of the mouth of the middle
distributor will not form the particles which are not completely
plasticized into the cavity, and then the inside of the bottle will be
made. There are unablated particles.
5, color
Color
questioning is said for colored bottles, such as green tea bottles are
light green. At this time, you need to pay attention to whether the
color is normal. The depth of the color has a certain scale, and it
depends on the distinction between the two eyes. Colors above or below
the color scale are abnormal colors. Anomalous color is usually an
abnormal operation of the masterbatch, perhaps an abnormality when the
screw is rotated and mixed.
6, the bottom bias
Bottom
deviation means that the injection molding point does not coincide with
the middle of the blow molding, so that the thickness near the bottle is
not uniform. There are many reasons for this. The common reasons are as
follows: The first thing may be that the injection mold itself is not
good enough, so that the thickness of the preform is not uniform. The
second possibility is that during the heating process, the preform is
not uniformly heated, and the stretching time is not uniform. The third
is the blow molding process stretching rod to reduce the skew.
7, fluorescent
Fluorescence
is usually presented along with the bottom bias, which means that the
screen is too thin to be investigated under the light, and some areas
are white and shiny. Such an appearance becomes fluorescent. The reason
for the fluorescence composition is similar to the bottom bias. It is
often present at the bottom and shoulders of the bottle, and sometimes
the excessive pressure of the blown air will also constitute
fluorescence.
8, bubbles
There are air bubbles inside the
automatic blow molding machine. The reason for the composition is that
the boring time is boring and insufficient, so that the plasticized
material contains gas.
9, other
The bottle is sometimes white,
opaque, and the appearance of the ring is raised. Usually the
composition of these shortcomings is comparatively summarized and is not
commonly described.
Phone:(+86)13901569990 / (+86)13962250904
E-mail: salesnj@kingswel.com
Fax: 0512-58686638
Address:1 Yuefeng Rd, Zhangjiagang, Jiangsu,China (Zhangjiagang Economical DevelopmentZone, Zhangjiagang, Jiangsu, China)